  • Corrosion fatigue — is fatigue in a corrosive environment. It is the mechanical degradation of a material under the joint action of corrosion and cyclic loading. Nearly all engineering structures experience some form of alternating stress, and are exposed to harmful …   Wikipedia

  • Corrosion — v · d · e Materials failure modes Buckling · …   Wikipedia

  • Environmental stress fracture — In materials science, environmental stress fracture or environment assisted fracture is the generic name given to premature failure under the influence of tensile stresses and harmful environments of materials such as metals and alloys,… …   Wikipedia

  • Pitting corrosion — Pitting corrosion, or pitting, is a form of extremely localized corrosion that leads to the creation of small holes in the metal. The driving power for pitting corrosion is the depassivation of a small area, which becomes anodic while an unknown… …   Wikipedia

  • Crevice corrosion — refers to corrosion occurring in confined spaces to which the access of the working fluid from the environment is limited. These spaces are generally called crevices. Examples of crevices are gaps and contact areas between parts, under gaskets or …   Wikipedia

  • Environmental stress cracking — (ESC) is one of the most common causes of unexpected brittle failure of thermoplastic (especially amorphous) polymers known at present. Environmental stress cracking may account for around 15 30% of all plastic component failures in service.H. F …   Wikipedia

  • Sulfide stress cracking — Sulfide stress cracking, or sulfide stress corrosion cracking (SSCC), is a special corrosion type, a form of stress corrosion cracking. Susceptible alloys, especially steels, react with hydrogen sulfide, forming metal sulfides and elementary… …   Wikipedia

  • Intergranular corrosion — (IGC), also termed intergranular attack (IGA), is a form of corrosion where the boundaries of crystallites of the material are more susceptible to corrosion than their insides. ( Cf. transgranular corrosion.)This situation can happen in otherwise …   Wikipedia

  • Brazing — This article is about the metal joining process. For the cooking technique, see braising. Brazing practice Brazing is a metal joining process whereby a filler metal is heated above and distributed between two or more close fitting parts by… …   Wikipedia

  • metallurgy — metallurgic, metallurgical, adj. metallurgically, adv. metallurgist /met l err jist/ or, esp. Brit., /meuh tal euhr jist/, n. /met l err jee/ or, esp. Brit., /meuh tal euhr jee/, n. 1. the technique or science of working or heating metals so as… …   Universalium

  • Ceramic matrix composite — Fracture surface of a fiber reinforced ceramic composed of SiC fibers and SiC matrix. The fiber pull out mechanism shown is the key to CMC properties …   Wikipedia